Toroidal-shaped magnetodielectric core for transformers and inductors manufacturing.
Material: Mo-permalloy
Initial permeability: 60µ
Loss tangent: 5.9·10-3 (H=72A/m, f=30kHz)
12·10-3...12.9·10-3 (H=24...72A/m, f=100kHz)
Shape: toroidal with fillet at one side
Dimensions: outer diameter 44mm
inner diameter 28mm
thickness 7.2mm
fillet radius: 4mm